PRODUCT SUPPORT PROGRAM FOR REPAIRING WELD CRACKS ON B, CB, DB, AND TB BUCKETS FOR CERTAIN 320D, 323D, 324D, 325D, AND 330D EXCAVATORS Caterpillar


`
PRODUCT SUPPORT PROGRAM FOR REPAIRING WELD CRACKS ON B, CB, DB, AND TB BUCKETS FOR CERTAIN 320D, 323D, 324D, 325D, AND 330D EXCAVATORS [REBE4613]
WORK TOOLS
BUCKET GP
PRODUCT SUPPORT PROGRAM FOR REPAIRING WELD CRACKS ON B, CB, DB, AND TB BUCKETS FOR CERTAIN 320D, 323D, 324D, 325D, AND 330D EXCAVATORS
REBE4613-02

26Nov2008
(Revised 10Mar2009)


M450
X151
X157
X260

 
After Failure Only
 (Limited distribution) 
  

PRODUCT SUPPORT PROGRAM FOR REPAIRING WELD CRACKS ON B, CB, DB, AND TB BUCKETS FOR CERTAIN 320D, 323D, 324D, 325D, AND 330D EXCAVATORS

6503
PS51596
NOTE:

This Program can only be administered after a failure occurs. The decision whether to apply the Program is made by the dealer. When reporting the repair, use "PS51596" as the Part Number and "7755" as the Group Number. Use "96" as the Warranty Claim Description Code and use "Z" as the SIMS Description Code.

NOTE:

The information supplied in this service letter may not be valid after the termination date of this program. Do not perform the work outlined in this Service Letter after the termination date without first contacting your AVSpare product analyst.

 
NOTE:

This Revised Service Letter replaces the 26Nov2008 (Revised 16Jan2009) Service Letter. Changes have been made to various parts of this Service Letter to note the inclusion of the "B" linkage buckets that were already included in the Affected Product.


TERMINATION DATE

30Nov2010

PROBLEM

The existing bucket hinge and top plate assembly on B, CD, DB, and TB Buckets can experience weld cracking on certain 323D, 324D, 325D, and 330D Excavators. If the existing hinge or top plate has weld cracks, it will need to be repaired and reworked.

AFFECTED PRODUCT

Model Identification Number
320D  DHK00199, 205, 212, 219, 229, 244, 248, 250, 253, 255, 327, 329-330, 332, 335, 342, 344, 347-348, 350-353, 355-358, 360-362, 365, 370, 373-375, 377, 387-389, 391-392, 395, 397-398, 400-401, 403-404, 406, 450, 452-453, 460-464, 475, 482, 537, 564, 568-569, 571, 575-580, 597, 600-601, 605, 628, 630, 759, 809, 889, 899-903, 906-909, 958, 965, 970-978, 985, 994
323D L BYM00317, 342, 357

PBM00224-00225, 315-316, 319, 323, 338-339, 342, 361-362, 371, 377-378, 384-385, 389, 392-393, 399, 402, 417, 420, 478-479, 482, 495, 498, 505-508, 514

SDC00271, 274, 279-280, 301, 315, 330, 342, 379, 392, 400, 445, 482, 494-495, 505, 509
323D LN CYD00326, 341, 482, 517

RAC00292, 369, 373, 391, 394, 402, 411, 431, 501, 516, 519, 531, 544
324D L  SYM00169, 174, 178, 180, 190, 214, 216, 221, 223-224, 228, 233, 271-272, 274-275, 277, 288, 296-300, 302-303, 305-306, 308-309, 312-313, 315-316, 319, 323-325, 328, 331-333, 339, 341-343, 348, 352-353, 362, 365, 367, 427-433, 450, 452-455, 473-478, 532-534, 541, 544-545, 599, 601, 603, 618-626, 628-629, 631, 633-637, 645, 664-668, 670-671, 676-677, 694-695, 697, 699, 701-702, 706-707, 722, 724, 731, 742, 751-753, 755-758, 764, 768, 771-774, 777-778
325D GPB00239-00240, 256, 261, 265, 273, 276, 279, 284-285, 288-289, 293, 299, 302, 305, 307, 317, 321, 327, 338, 344-345, 347-349, 351, 353, 376, 379, 381, 387-391, 404, 406, 413, 415-416, 418-419, 426, 430-431, 433-435, 438, 441-442, 444-445, 457, 466, 471, 477-479, 481, 486, 497, 564, 568, 579, 582, 584-592, 602-604, 611, 616-618, 624-625, 650-653, 655, 674, 677-678, 680, 682, 734, 757, 805-806, 808-814, 816, 846-849, 853-854, 858-869, 886, 900-901, 910, 912-915, 926-928, 944, 948, 961, 963-965, 967-968, 981, 992, 1012-1015, 1046-1048, 1052-1055, 1064, 1066-1073

PKE00206, 470, 524, 847
325D L  MCL00151
330D GGE00354, 418, 694, 751, 753

RAS00175-00176, 200-207, 210, 212, 215, 217, 219, 222, 226, 228-233, 236-237, 239-240, 242, 245, 249-250, 264, 268, 274-276, 280-283, 285-287, 289, 291, 293-294, 301, 305, 319, 326, 328, 338, 341-343, 351, 393, 399, 405-407, 412-413, 415, 417-418, 420, 426, 428, 432-433, 437-438, 440, 442, 453-456, 469, 471-476, 479, 481, 494, 498, 500-501, 503-504, 513, 521-522, 581-583, 587-590, 597, 609-610, 614, 616-619, 626, 628, 650, 680, 682-685, 687-689, 700, 712, 734, 739, 744, 756-758, 770, 772, 776-777, 787, 793, 795, 800, 803, 815, 820, 824-825, 827, 829, 831-832, 849, 851, 853, 899-900, 911-913, 915, 917-919, 930-931, 937-939, 941-942, 944-945, 947, 973, 992-1000, 1004, 1019, 1023, 1025, 1055, 1059-1060, 1075, 1089-1090, 1092-1093, 1103, 1143-1146, 1155-1156, 1161, 1165-1168, 1170-1172, 1174-1176, 1181, 1184, 1192, 1198, 1207, 1209, 1213, 1215-1217, 1219-1222, 1234-1236, 1242, 1244-1245, 1248-1250, 1253-1256, 1258-1262, 1264, 1268-1269, 1272, 1275, 1277, 1279-1280, 1289, 1297

THJ00241-00244, 256-257, 260, 275, 277-280, 283

PARTS NEEDED

No parts needed for this program

ACTION REQUIRED

Refer to Special Instruction, REHS3874, for the rework procedure for weld cracking on B, CB, DB, and TB Buckets.

SERVICE CLAIM ALLOWANCES

Product smu/age whichever comes first
AVSpare
Dealer Suggested
Customer Suggested
Parts %
Labor Hrs%
Parts %
Labor Hrs%
Parts %
Labor Hrs%
0-24 mo 
100.0%
100.0%
0.0%
0.0%
0.0%
0.0%
 NOTE: This is a 10.0-hour job



PARTS DISPOSITION

Handle the parts in accordance with your Warranty Bulletin on warranty parts handling.
 
 
 


Rework Procedure


 
A rework procedure for B, CB, DB and TB buckets is now available for the cracking of certain welds that are located on the top plate assembly of the bucket. The rework procedure describes the repair process for certain excavator buckets. Refer to Special Instruction, REHS3874, "Rework Procedure for Weld Cracks of B, CB, DB and TB Buckets for Certain Excavators".

Dealers need to supply and fabricate steel plates per Special Instruction, REHS3874. Use structural steel ASTM A572 or equivalent. The length and thickness of the steel plate will vary depending upon the bucket. There are no additional required parts for the rework process.
 
 

Information System:

PRODUCT SUPPORT PROGRAM FOR REPLACING THE 286-4201 TUBE ASSEMBLY ON CERTAIN 414E INDUSTRIAL LOADERS
PRODUCT IMPROVEMENT PROGRAM FOR INSTALLING THE LEVELING SWITCH AND/OR REPLACING, IF NECESSARY, THE LEVELING VALVE GROUP ON CERTAIN 323DL EXCAVATORS
PRODUCT SUPPORT PROGRAM FOR MODIFYING CERTAIN PIN GRABBER PERFORMANCE BUCKETS FOR USE WITH CERTAIN DB, B, AND 315 LINKAGE PIN GRABBER COUPLERS
PRODUCT IMPROVEMENT PROGRAM FOR REMOVING 7Y-4945 AND 087-5550 BACK-UP RINGS FROM DEALER PARTS STOCK
PRODUCT IMPROVEMENT PROGRAM FOR INSPECTING, AND REWORKING IF NEEDED, THE MAIN HYDRAULIC PUMP REGULATOR ON CERTAIN 385C, 385CL, 385CL MH AND 385C FS EXCAVATORS
PRODUCT SUPPORT PROGRAM FOR REWORKING THE HYDRAULIC SWING MOTOR ON CERTAIN 330C, 330C L, 330D, AND 330D L EXCAVATORS
PRODUCT SUPPORT PROGRAM FOR REPLACING THE MAIN PUMP ON CERTAIN 320D, 320DL, 324D, 324DL, 325D EXCAVATORS AND 950H, 962H, 966H, 972H WHEEL LOADERS
PRODUCT SUPPORT PROGRAM FOR REPLACING THE FAN DRIVE PULLEY AND THE CRANKSHAFT PULLEY ON CERTAIN 308D MINI HYDRAULIC EXCAVATORS
PRODUCT IMPROVEMENT PROGRAM FOR REPLACING LOWER COMPACTOR ASSEMBLY ON CERTAIN CVP40 VIBRATORY PLATE COMPACTORS
PRODUCT SUPPORT PROGRAM FOR REWORKING THE HYDRAULIC SWING MOTOR ON CERTAIN 330C L, 330D L, AND 336D L EXCAVATORS
PRODUCT IMPROVEMENT PROGRAM FOR FLASHING NEW SOFTWARE AND REPLACING FUEL FILTERS ON CERTAIN 320D EXCAVATORS EQUIPPED WITH C6.4 ENGINES
PRODUCT IMPROVEMENT PROGRAM FOR REMOVING ALL 260-3010 SEAL KITS FROM DEALER PARTS STOCK
PRODUCT IMPROVEMENT PROGRAM TO CEASE OPERATION, INSPECT, AND REPLACE IF NEEDED, THE BOOM CYLINDERS ON CERTAIN 330D EXCAVATORS
PRODUCT IMPROVEMENT PROGRAM FOR RE-TIGHTENING THE 292-7595 OR 292-7590 TUBE ASSEMBLY ON CERTAIN 319D L AND 319D LN EXCAVATORS
PRODUCT SUPPORT PROGRAM FOR REPLACING THE PIN ASSEMBLIES ON CERTAIN 330D AND 336D EXCAVATORS
PRODUCT SUPPORT PROGRAM FOR REPLACING THE BUCKET CYLINDER PISTON ON CERTAIN 416E, 422E, 428E, 432E, AND 434E BACKHOE LOADERS
PRODUCT SUPPORT PROGRAM TO REPLACE THE 194-0820 BLOCK ON CERTAIN 330D L, 336D L, AND 330D MH FCR EXCAVATORS
PRODUCT SUPPORT PROGRAM FOR REWORKING THE ALL WHEEL STEER SYSTEM ON CERTAIN 432E, 434E, 442E AND 444E BACKHOE LOADERS
PRODUCT SUPPORT PROGRAM FOR REPLACING THE STEERING CYLINDER ON CERTAIN 414E, 416E, 420E, 422E, 428E, 430E, 432E, AND 442E BACKHOE LOADERS
PRODUCT IMPROVEMENT PROGRAM FOR INSPECTING THE CYLINDER HEAD LIFTING EYE BOLT HOLE ON VARIOUS 3508, 3512, AND 3516 ENGINES
PRODUCT SUPPORT PROGRAM FOR INSTALLING THE CAB AIR DUCT ASSEMBLIES ON CERTAIN 321D AND 328D EXCAVATORS
PRODUCT IMPROVEMENT PROGRAM FOR INSPECTING THE HYDRAULIC CYLINDER RODS ON CERTAIN 319D EXCAVATORS
PRODUCT IMPROVEMENT PROGRAM FOR INSPECTING THE MAIN CONTROL VALVE ON CERTAIN 345C, 345CL, 345D AND 345DL EXCAVATORS
PRODUCT SUPPORT PROGRAM TO INSPECT AND REPLACE THE FUEL HOSE CONDUIT ON CERTAIN 345D L EXCAVATORS